Аннотация
Nickel oxide nanopowder was prepared by a simple method and analyzed by
X-ray powder diffraction. A solution of gelatin and NiCl2 center dot
6H(2)O salt were prepared and sintered in sequence. Using a synchrotron
light source for X-ray powder diffraction analysis, the synthesized
material was characterized as a function of temperature in the interval
of 375 to 600 degrees C. Results from thermogravimetric analysis confirm
the temperature loss of the organic substance during the sintering
process and show that the temperature for NiO attainment is 600 degrees
C. (C) 2008 International Centre for Diffraction Data.